Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on the Mechanical Characteristics by the Change of Bevel Angle of Welding Joint during PWHT

Journal of KWJS 1997;15(2):64-71.
Published online April 25, 1997.
용접이음부 형태변화에 따른 후열처리시의 역학적 특성에 관한 연구
, , , ,
 
A Study on the Mechanical Characteristics by the Change of Bevel Angle of Welding Joint during PWHT
방한서, 강성원, 김기성, 김종명, 노찬승