Optimization of HVOF Spray Parameters for Cr3C2-7wt%NiCr Coating Powder by Experimental Design Method
김병희, 서동수

Correspondence:   Published online February 25, 1997
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,024
View
0
Download
Related articles
Optimization of Disk Laser Welding Parameters in Pure Ti Using Taguchi Method  2018 February;36(1)
Optimization of GTAW Parameters for Horizontal Welding of a STS316L Pipe  2015 October;33(5)
Optimization of arc brazing process parameters for exhaust system parts using box-behnken design of experiment  2015 April;33(2)
Optimization of Welding Parameters for Resistance Spot Welding of TRIP Steel using Response Surface Methodology  2003 April;21(2)
Optimization of the Plasma Spray Coating Parameters of Ni-5%AI Alloy Powder   2002 October;20(5)
Optimization of Disk Laser Welding Parameters in Pure Ti Using Taguchi Method  2018 February;36(1)
Optimization of GTAW Parameters for Horizontal Welding of a STS316L Pipe  2015 October;33(5)
Optimization of arc brazing process parameters for exhaust system parts using box-behnken design of experiment  2015 April;33(2)
Optimization of Welding Parameters for Resistance Spot Welding of TRIP Steel using Response Surface Methodology  2003 April;21(2)
Optimization of the Plasma Spray Coating Parameters of Ni-5%AI Alloy Powder   2002 October;20(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI