Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Effect of HAZ Softening Zone on Creep Rupture Propertes of 1.0Cr-1.0Mo-0.25V Turbine Rotor Steels - Part II : Carbide Morphology -

Journal of KWJS 1997;15(1):101-108.
Published online February 25, 1997.
1.0Cr-1.0Mo-0.25V 터어빈 로터강의 열영향부 연화층이 크립 파단 특성에 미치는 영향 - Part II : 탄화물 형태 -
,
 
Effect of HAZ Softening Zone on Creep Rupture Propertes of 1.0Cr-1.0Mo-0.25V Turbine Rotor Steels - Part II : Carbide Morphology -
오영근, J.E. Indacochea