Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2025-06.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 The Bonding Mechanism and Bond Strength of Cold Pressure Welding

Journal of KWJS 1990;8(3):31-38.
Published online September 25, 1990.
업셋팅에 의한 냉간 압접의 결합 기구와 결합강도
,
 
The Bonding Mechanism and Bond Strength of Cold Pressure Welding
한인철, 김재도