Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 Fatigue Properties of Welded Joints for TMCP Steels

Journal of KWJS 1990;8(2):40-52.
Published online June 25, 1990.
TMCP 고장력강 용접부의 피로 특성에 관한 연구
, , ,
 
Fatigue Properties of Welded Joints for TMCP Steels
임채범, 권영각, 장래웅, 엄기원