Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-03.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Laser Additive Manufacturing Technology Review

J Weld Join > Volume 32(4); 2014 > Article
Journal of Welding and Joining 2014;32(4):353-357.
DOI: https://doi.org/10.5781/JWJ.2014.32.4.15    Published online August 30, 2014.
Laser Additive Manufacturing Technology Review
Myun Joong Hwang*, Jungho Cho**
Correspondence:  Jungho Cho,
Email: Junghocho@cbnu.ac.kr
Abstract
Additive manufacturing technology is taking great attentions in these days because the term 3D-printing became a hot issue as the next generation manufacturing paradigm. Especially, laser additive manufacturing is at the center of interest thanks to the accuracy compared to other heat sources. In this report, recent papers about laser additive manufacturing are analyzed and reviewed. General technology is specified into three different categories and they are laser sintering, laser melting and laser metal deposition. Similarities and differences are clearly described by detailed technologies and used materials type. Representative application examples are selected then future of this technology is expected through those applications. Additionally, market of laser additive manufacturing systems itself and application fields are also predicted based on present 3D-printing market and technical progressions.
Key Words: Additive manufacturing, Laser sintering, Laser metal deposition


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI