Journal of Welding and Joining 2014 February;32(1) :34-39.
Published online February 27, 2014.
doi:https://doi.org/10.5781/JWJ.2014.32.1.34
FSW Properties of Aluminum alloy 5000/6000 for Small Boat
Je-Hyoung Cho*, Myung-Hyun Kim**, Jun-Woong Choi*
*Research Institute of Medium & Small Shipbuilding, Busan 618-270, Korea
**Naval Architecture & Ocean Engineering, Pusan National University, Busan 609-735, Korea
Correspondence: Je-Hyoung Cho  Email: jhcho@rims.re.kr
  Published online February 27, 2014
ABSTRACT
There are so many difficulties of melt bonding mainly applied for hull construction of a aluminum alloy small boat. For resolving this problem, Friction stir welding(FSW) in non-melting solid state welding Process generally is applied in the transport industry. This paper is studied the joining strength characteristics and macrostructure according to dissimilar aluminium 5000/6000 alloy joining for a small boat applied for this FSW technology. It is reported that difference of joining strength in accordance with the direction of rotation in case of friction stir welding between dissimilar metals(Al/Cu, Al/Fe) is also highly large. In this study, Test is carried out by making the specimen according to the direction of rotation of dissimilar aluminium alloy joining.
Keywords: Friction Stir Welding | Dissimilar aluminium alloy | Joining-characteristics | Macrostructure | Small Boat | Aluminum 5000 alloy | Aluminum 6000 alloy
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
2,064
View
31
Download
Related articles
Flame Braze between Aluminum Alloy 5A06 and Low Carbon Steel Q235   2017 August;35(4)
Application of Friction Stir Welding Processes for Aluminum alloy Boat  2012 April;30(2)
Weldabilities of 7000 Aluminium Alloys ( III )   1994 September;12(3)
Weldabilities of 7000 Aluminium Alloys ( II )   1994 June;12(2)
Weldabilities of 7000 Aluminium Alloys ( I )   1994 March;12(1)
Flame Braze between Aluminum Alloy 5A06 and Low Carbon Steel Q235   2017 August;35(4)
Application of Friction Stir Welding Processes for Aluminum alloy Boat  2012 April;30(2)
Weldabilities of 7000 Aluminium Alloys ( III )   1994 September;12(3)
Weldabilities of 7000 Aluminium Alloys ( II )   1994 June;12(2)
Weldabilities of 7000 Aluminium Alloys ( I )   1994 March;12(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI