Application of Friction Stir Welding Processes for Aluminum alloy Boat
Je-Hyoung Cho, Myung-Hyun Kim, Jun-Woong Choi


Correspondence:   Published online May 16, 2012
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,632
View
0
Download
Related articles
A Review on the Design Rule for the Friction Stir Welding using Bobbin Tool for Aluminum  2021 October;39(5)
Review and Feasibility Study on Micro Friction Stir Welding of Al/Fe Butt Joints  2021 June;39(3)
Optimization of Friction Stir Welding Parameters of AA2014-T6 Alloy using Taguchi Statistical Approach  2020 October;38(5)
Optimization of PWHT on Dissimilar Friction Welding for Piping Material of A105 to A312  2019 April;37(2)
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
A Review on the Design Rule for the Friction Stir Welding using Bobbin Tool for Aluminum  2021 October;39(5)
Review and Feasibility Study on Micro Friction Stir Welding of Al/Fe Butt Joints  2021 June;39(3)
Optimization of Friction Stir Welding Parameters of AA2014-T6 Alloy using Taguchi Statistical Approach  2020 October;38(5)
Optimization of PWHT on Dissimilar Friction Welding for Piping Material of A105 to A312  2019 April;37(2)
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI