Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2025-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 Effects of Tool Speed on Joining Characteristics during Friction Stir Spot Welding of Mg-alloy(AZ31B) Sheet

Journal of KWJS 2011;29(2):80-87.
Published online May 7, 2011.
마그네슘합금(AZ31B) 판재의 마찰교반 점용접시 접합특성에 미치는 툴 속도의 영향
, ,
 
Effects of Tool Speed on Joining Characteristics during Friction Stir Spot Welding of Mg-alloy(AZ31B) Sheet
Hyung-Seop Shin, Yoon-Chul Jung, Kwang Choi
Abstract
  In this study, the friction stir spot welding (FSSW) of Mg alloy sheets has been tried using an apparatus devised with a CNC milling machine to give the precise control of joining condition including tool speed. The probe tool used is made of hard metal and composed of cylindrical shoulder and pin parts. The variation of morphologies formed after the friction stir spot welding depending on the plunge speed of the tool were investigated at each rpm of tool. The history of the temperature distribution and the vertical load induced during the spot welding with friction time were measured by using an Infrared Thermal Imager (THERMA CAMTM SC2000) and a loadcell located below the specimen fixture, respectively. Tensile-shear tests were also performed to evaluate the fracture load of welded specimens. In order to characterize the friction stir spot welding of Mg alloy sheets, the variation of the fracture load was discussed on micrographic observations, temperature distribution during the FSSW according to the plunge speeds of tool.
Key Words: Friction stir spot welding (FSSW), Mg alloy (AZ31B), Tool speed, Joining characteristics, Tensile-shear test


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2025 by The Korean Welding and Joining Society.

Developed in M2PI