Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-07.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 Weld Quality Quantification through Chaotic Analysis

Journal of KWJS 2010;28(1):72-76.
Published online March 10, 2010.
카오스 분석을 통한 용접 품질 정량화
, ,
 
Weld Quality Quantification through Chaotic Analysis
Jung-Ho Cho, Dave Farson, Cheolhee Kim
Abstract
  Irregular fluctuation of penetration depth in CW single mode fiber laser welding is analyzed statistically and chaotically. Among various chaos theories, one of the basic concept referred as Lyapunov exponent is applied to the analysis to quantify the irregularity of penetration. Especially, maximal Lyapunov exponent (MLE) is known as the representative value indicating chaotic degree of the system dynamics. MLE calculation method of experimental data is applied to longitudinal spiking defect in fiber laser weld. Laser power modulation is suggested as a remedy then the computed MLE value is compared to CW case. It is shown that the adoption of chaos theory, MLE computation, can be used as a measurement standard to prove the validity of the solutions to prevent the unexpected chaotic behavior of weld through this work.
Key Words: Fiber laser, Welding, Chaos, Lyapunov exponent, Spike
TOOLS
METRICS Graph View
  • 1,722 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI