A Study on the Mechanical Properties of MAG Weld on Ferritic Stainless Steel Sheets
Gyeong-cheol Lee, Jae-seong Kim, Hyun-jae Kim, Kyoung-ho Lim, Bo-Young Lee




Correspondence:   Published online May 18, 2009
ABSTRACT
  Ferritic stainless steels have a good heat resistance and economic advantage. They are used for pplications such as automotive exhaust systems where resistance to general corrosion is superior to carbon teels. However, there are not enough research for ferritic stainless steels on weldability mainly used as utomotive exhaust manifolds. In this study, mechanical and microstructure properties of as-welded STS 29L and STS 444 ferrite stainless steels were confirmed by tensile, bending, hardness test, optical icroscopy and scanning electron microscopy. Tensile strength of the STS 444 is higher than the STS 29L when it is a raw material. In contrast to this fact, STS 429L indicated higher tensile strength after utt welded. In addition, the hardness have a increasing tendency as getting down on the bead.
Keywords: GMAW;MAG;Weldability;Ferritic stainless steel;STS 429L;STS 444;Solid wire STS430LNb
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,644
View
0
Download
Related articles
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 December;37(6)
Microstructure and Mechanical Properties of Friction-Welded Alloy 718 and SNCRW Stainless Steel After Post-Weld Heat-Treatment  2019 August;37(4)
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 August;37(4)
Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels  2018 October;36(5)
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 December;37(6)
Microstructure and Mechanical Properties of Friction-Welded Alloy 718 and SNCRW Stainless Steel After Post-Weld Heat-Treatment  2019 August;37(4)
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 August;37(4)
Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels  2018 October;36(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI