Development of Thermal Distortion Analysis Method Based on Inherent Strain for TMCP Steels
Yunsok Ha, Jinhyuk Yang, Seokhee Won, Myungsu Yi



Correspondence:   Published online July 31, 2008
ABSTRACT
  As ships become to be larger than ever, the thicker plate and the higher tensile steel plate are used in naval shipyard. Though special chemical composition is needed for high-tensile steels, recent high-tensile steels are made by the TMCP(Thermo-Mechanical control process) skill. The increase of yield stress and tensile stress of TMCP steels is induced from bainite phase which is transformed from austenite, but that increased yield stress can be vanished by another additional thermal cycle like welding and heating. As thermal deformations are deeply related by yield stress of material, the study for prediction of plate deformation by heating should reflect principle of TMCP steels. This study developed an algorithm which can calculate inherent strain. In this algorithm, not only the mechanical principles of thermal deformations, but also the predicting of the portion of initial bainite is considered when calculating inherent strain. The simulations of plate deformation by these values showed good agreements with experimental results of normalizing steels and TMCP steels in welding and heating. Finally we made an inherent strain database of steels used in Class rule.
Keywords: Inherent strain;TMCP;Bainite;Thermal elastic-plastic analysis;Yield stress
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,353
View
0
Download
Related articles
Thermal Deformation Analysis Methodology Development for Inconel Overlaying  2022 April;40(2)
Development of Quality Inspection System for Fillet Welding Based on Laser Vision Sensor  2018 December;36(6)
A Study on the Thermal Distortion Analysis of Welded Structures having K/X Groove using shell elements  2012 December;30(6)
Development of Welding Quality Monitoring Method for TIG Cladding  2013 December;31(6)
Development of Distortion Analysis Method for Multi-pass Butt-welding Based on Shell Element  2010 February;28(1)
Thermal Deformation Analysis Methodology Development for Inconel Overlaying  2022 April;40(2)
Development of Quality Inspection System for Fillet Welding Based on Laser Vision Sensor  2018 December;36(6)
A Study on the Thermal Distortion Analysis of Welded Structures having K/X Groove using shell elements  2012 December;30(6)
Development of Welding Quality Monitoring Method for TIG Cladding  2013 December;31(6)
Development of Distortion Analysis Method for Multi-pass Butt-welding Based on Shell Element  2010 February;28(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI