Effects of Process Parameters on Friction Stir Weldability in Dissimilar Joints of AA5052 and Advanced High Strength Steel
Hee-Seon Bang*, Han-Sur Bang*, Kyoung-Hak Kim*
*Dept. of Welding and Joining Science Engineering, Chosun University, Gwangju, 61452, Korea
Correspondence: Kyoung-Hak Kim  Email: kimkh@chosun.kr
Received October 5, 2020  Revised November 4, 2020  Accepted February 8, 2021  Published online April 2, 2021
ABSTRACT
The dissimilar joining of aluminum (Al) alloy and steel has become attractive in the automotive sector to achieve lightweight components. However, joining Al to steel using conventional fusion welding processes is difficult because of their widely varying thermo-physical properties and the formation of intermetallic compounds (IMCs) at the Al-Fe joint interface. In the present study, the dissimilar joining of a 2.5 mm thick AA5052-H32 and a 1.4 mm thick DP590 steel sheet was performed using friction stir welding (FSW). Moreover, the effects of the process parameters on the mechanical properties and microstructure of FS welds was investigated. The tensile test results indicated that a higher heat input with increasing rotation speed and decreasing travel speed contributed to a higher tensile strength. The maximum tensile strength of the FS welds was 178 MPa, which exhibited a joint efficiency of approximately 79%. As a result of scanning electron microscopy (SEM) with energy dispersive spectrometry (EDS) and X-ray diffraction (XRD) analysis, a thin interfacial layer of less than 1 μm thickness comprising Fe4Al13 IMC was observed at the dissimilar Al-Fe joint interface.
Keywords: Friction stir welding | Dissimilar Al/steel joints | Mechanical properties | Microstructure | Fracture behavior
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
176
View
48
Download
Related articles
Effect of Process Parameters on the Formation of Lack of Fusion in Directed Energy Deposition of Ti-6Al-4V Alloy  2019 December;37(6)
Effect of Circumferential Tool Path Control on Friction Stir Spot Welding of Al/Fe Dissimilar Metal Joint  2016 June;34(3)
Expulsion of Electric Resistance Spot Welding in Advanced High Strength Steels for Automobile  2011 December;29(6)
Recent Studies on Friction Stir Welding of High Carbon Steels  2009 October;27(5)
Effects of Nd:YAG Laser Welding Parameters on Fatigue life of Lap Joint Structure in Stainless Steel  2008 February;26(1)
Effect of Process Parameters on the Formation of Lack of Fusion in Directed Energy Deposition of Ti-6Al-4V Alloy  2019 December;37(6)
Effect of Circumferential Tool Path Control on Friction Stir Spot Welding of Al/Fe Dissimilar Metal Joint  2016 June;34(3)
Expulsion of Electric Resistance Spot Welding in Advanced High Strength Steels for Automobile  2011 December;29(6)
Recent Studies on Friction Stir Welding of High Carbon Steels  2009 October;27(5)
Effects of Nd:YAG Laser Welding Parameters on Fatigue life of Lap Joint Structure in Stainless Steel  2008 February;26(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI