Advanced Search  
JWJ > Volume 39(2); 2021 > Article
Journal of Welding and Joining 2021 April;39(2) :144-149.
Published online April 23, 2021.
doi:https://doi.org/10.5781/JWJ.2021.39.2.2
Residual Stress Study of High Manganese Steel Riser Pipe Manufactured by Longitudinal Butt Welding (2) : Equation for Predicting Welding Induced Residual Stresses Established through Parametric Study
Myung-Su Yi*, Jung-Kwan Seo**,***
*Faculty of Smart Vehicle System Engineering, Chosun University, Gwangju, 61452, Korea
**,***Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Korea
The Korea Ship and Offshore Research Institute (The Lloyd’s Register Foundation Research Centre of Excellence), Pusan National University, Busan, 46241, Korea
Correspondence: Myung-Su Yi  Email: true413@chosun.ac.kr
Received April 4, 2021  Revised April 13, 2021  Accepted April 20, 2021  Published online April 23, 2021
ABSTRACT
In recent years, the deep and ultra-deep seas are recognized as the last remaining regions on the planet where oil and natural gas resources are discovered and produced. In order to develop such natural resources in an environmentally safe and cost-effective method, various engineering systems and technologies are being developed. In keeping with this direction of development, there is significant worldwide interest among major offshore structural and system operators in examining the possibility of using high-strength steel for long-distance gas transmission pipelines and risers. In particular, riser pipes using high manganese steel are often made by longitudinal butt welding, but studies related to the prediction of residual stresses for this are insufficient. In general, it is known that in a cylindrical structure such as steel catenary risers (Hereafter, ‘SCRs’), residual stress in the through-thickness direction can be decomposed into a membrane component and a bending component. In this paper, a parametric study through nonlinear finite element analysis was performed to predict the residual stress for each direction of a longitudinal butt-welded riser by considering the main parameters (r/t) of the pipe that can affect the actual residual stress. A new predicting equation for estimating the residual stress profile was proposed using the results of a number of parametric precision numerical analysis derived through this process.
Keywords: Riser | High manganese steel | Longitudinal butt welding | Residual stress | FEA | Parametric study | Through-thickness | Membrane stress | Bending stress | Self-equilibrium stress | Empirical formulae
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
106
View
11
Download
Related article
Residual Stress Study of High Manganese Steel Riser Pipe Manufactured by Longitudinal Butt Welding (1) : Residual Stress Measurement and FE Analysis  2021 April;39(2)
Residual Stress Study of High Manganese Steel Riser Pipe Manufactured by Longitudinal Butt Welding (1) : Residual Stress Measurement and FE Analysis  2021 April;39(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI