Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Precipitation and Precipitate Coarsening Behavior According to Nb Addition in the Weld HAZ of a Ti-containing Steel
Joonoh Moon, Changhee Lee
JWJ. 2008;26(1):76-82.   Published online 2008 March 21

Excel Download

Influence of Nb addition on the particle coarsening and microstructure evolution in a Ti-containing steel weld HAZ
Materials Science and Engineering: A. 2007;454-455:648-653   Crossref logo
Link1 Link2

HAZ softening in Nb-, Ti- and Ti + V-bearing quenched and tempered steel welds
Welding in the World. 2016;60(2):177-184   Crossref logo
Link1 Link2 Link3

Impact of Precipitate Morphology on the Dissolution and Grain-Coarsening Behavior of a Ti-Nb Microalloyed Linepipe Steel
Metals. 2020;10(1):89   Crossref logo
Link1

Coarsening Behavior of the (Ti, Nb)(C, N) Complex Particle in a Microalloyed Steel Weld Heat-Affected Zone Considering the Critical Particle Size
Metallurgical and Materials Transactions A. 2007;38(11):2788-2795   Crossref logo
Link1 Link2 Link3

Microstructure and precipitation behavior in HAZ of V and Ti microalloyed steel
Journal of Iron and Steel Research International. 2009;16(3):68-72   Crossref logo
Link1 Link2 Link3 Link4 Link5

Strain-Induced Precipitation Behavior of a Nb-Ti-V Steel in the Austenite Phase Field
steel research international. 2013;84(9):827-836   Crossref logo
Link1 Link2

On Control of Grain Coarsening of Austenite by Nano-Scale Precipitate Engineering of TiN-NbC Composite in Ti-Nb Microalloyed Steel
Proceedings of the 6th International Conference on Recrystallization and Grain Growth (ReX&GG 2016). 2016;119-124   Crossref logo
Link1

Coarsening kinetics of TiN particle in a low alloyed steel in weld HAZ: Considering critical particle size
Acta Materialia. 2006;54(4):1053-1061   Crossref logo
Link1 Link2

Creep and fracture behavior of long-annealed weld HAZ in CB2 steel
Welding in the World. 2020;64(3):573-590   Crossref logo
Link1 Link2 Link3

Behavior of (Ti, Nb)(C, N) complex particle during thermomechanical cycling in the weld CGHAZ of a microalloyed steel
Acta Materialia. 2009;57(7):2311-2320   Crossref logo
Link1 Link2