Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Development of an Algorithm for Controlling Welding Bead Using Infrared Thermography
김일수, 박창언, 손준식, 박순영, 정영재, Yarlagadda Prasad
J Weld Join. 2000;18(6):55-61.   Published online 2000 December 25

Excel Download

Development of an Artificial Intelligence Powered TIG Welding Algorithm for the Prediction of Bead Geometry for TIG Welding Processes using Hybrid Deep Learning
Metals. 2020;10(4):451   Crossref logo
Link1

Drying behaviour of masonry using quantitative infrared thermography
Drying behaviour of masonry using quantitative infrared thermography. 2023;   Crossref logo
Link1

Spectrogram Based Detection Algorithm for Back-Bead in Gas Metal Arc Welding Process using Convolution Neural Network
Journal of Welding and Joining. 2021;39(2):198-205   Crossref logo
Link1 Link2 Link3

A Study on the Algorithm for Determining Back Bead Generation in GMA Welding Using Deep Learning
Journal of Welding and Joining. 2018;36(2):74-81   Crossref logo
Link1 Link2 Link3

Suitability of lock-in infrared thermography for luminescent glass development
Quantitative InfraRed Thermography Journal. 2019;17(2):96-106   Crossref logo
Link1

Algorithm of Infrared Camera Measurement Processing Path
Infrared Thermography. 2009;41-60   Crossref logo
Link1

A novel pulse compression algorithm for frequency modulated active thermography using band-pass filter
Infrared Physics & Technology. 2017;82:75-84   Crossref logo
Link1 Link2

Infrared thermography for monitoring the robotic welding process
NDT & E International. 1996;29(6):392   Crossref logo
Link1 Link2

Analysis of the accuracy of a neural algorithm for defect depth estimation using PCA processing from active thermography data
Infrared Physics & Technology. 2013;56:1-7   Crossref logo
Link1 Link2

Automatic Dispersion, Defect, Curing, and Thermal Characteristics Determination of Polymer Composites using Micro-Scale Infrared Thermography and Machine Learning Algorithm
. 2022;   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.