Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Solidification Crack Free Welding Strategy via Ultra High Precision Laser Scanning at a Single Grain of Directionally Solidified and Single Crystal Superalloys
Seong-Jin Lee, Kyeong-Min Kim, Heeshin Kang, Seong-Moon Seo, Wonah Park, Eun-Joon Chun
J Weld Join. 2023;41(4):254-264.   Published online 2023 August 31    DOI: https://doi.org/10.5781/JWJ.2023.41.4.4

Excel Download

Solidification Crack Free Welding Strategy via Ultra High Precision Laser Scanning at a Single Grain of Directionally Solidified and Single Crystal Superalloys
Journal of Welding and Joining. 2023;41(4):254-264   Crossref logo
Link1 Link2 Link3

Numerical Analysis of Nucleation and Growth of Stray Grain Formation during Laser Welding Nickel-Based Single-Crystal Superalloy Part II: Solidification Cracking Diminution through Single-Crystallinity Control
Solid State Phenomena. 2022;330:61-70   Crossref logo
Link1

Grain Optimization: Optimizing Grain Selection Design in the Single‐Crystal Solidification of Ni‐Based Superalloys (Crystal Research and Technology 12/2018)
Crystal Research and Technology. 2018;53(12):   Crossref logo
Link1 Link2

Numerical Analysis of Stray Grain Formation during Laser Welding Nickel-Based Single-Crystal Superalloy Part III: Crystallography-Dependent Solidification Behavior
Materials Science Forum. 2021;1033:40-48   Crossref logo
Link1

Solute segregation behavior of nickel-based single crystal superalloys directionally solidified under transverse static magnetic field
Materials Characterization. 2023;200:112914   Crossref logo
Link1 Link2

A new strategy to inhibit stray grain formation during laser directed solidification of single crystal superalloys
Journal of Alloys and Compounds. 2022;906:163852   Crossref logo
Link1 Link2

Erosion behaviour of platinum aluminide bond coat on directionally solidified CM247 and AM1 single crystal superalloys
Surface and Coatings Technology. 2022;429:127941   Crossref logo
Link1 Link2

Solidification morphologies in directionally solidified superalloys
Materials Science and Engineering. 1984;65(1):171-180   Crossref logo
Link1 Link2

Processing of directionally cast nickel-base superalloys: solidification and heat treatments
Nickel Base Single Crystals Across Length Scales. 2022;193-222   Crossref logo
Link1 Link2

Optimizing Grain Selection Design in the Single‐Crystal Solidification of Ni‐Based Superalloys
Crystal Research and Technology. 2018;53(12):   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.