Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Strategy of Suppressing the Solidification Cracking Susceptibility of 247LC Superalloy Weld Metals using Commercial Ni-Based Fillers |
Eun-Joon Chun |
J Weld Join. 2023;41(1):64-72. Published online 2023 February 21 DOI: https://doi.org/10.5781/JWJ.2023.41.1.7 |
Strategy of Suppressing the Solidification Cracking Susceptibility of 247LC Superalloy Weld Metals using Commercial Ni-Based Fillers Method of Suppressing Solidification Cracking by Laser Surface Melting and Epitaxial Growth Behavior for Directionally Solidified 247LC Superalloy Stray Grain Formation and Solidification Cracking Susceptibility of Single Crystal Ni-Base Superalloy CMSX-4 Variation of liquation cracking susceptibility for over–aged 247LC superalloy repair weld heat–affected zone Prediction of Cracking Susceptibility of Commercial Aluminum Alloys during Solidification Influence of laser powder bed fusion process parameters on the microstructure and cracking susceptibility of nickel-based superalloy Alloy 247LC Numerical Analysis of Aerospace Nickel-Based Single-Crystal Superalloy Weldability Part III: Solidification Cracking Susceptibility Solidification cracking in duplex stainless steel flux-cored arc welds Part 2 — susceptibility of 22Cr all-weld metals under high restraint Predicting Susceptibility to Solidification Cracking and Liquation Cracking by CALPHAD Effect of solidification models on predicting susceptibility of carbon steels to solidification cracking |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |