Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Analysis of Plasma Cutting Characteristics by the Vibration Signal of a Base Material |
Seonmin Kim, Dae-Won Cho, Seung-Hoon Bae, Upendra Tuladhar, Sang-Hyun Ahn |
J Weld Join. 2022;40(6):533-539. Published online 2022 December 30 DOI: https://doi.org/10.5781/JWJ.2022.40.6.9 |
Analysis of Plasma Cutting Characteristics by the Vibration Signal of a Base Material Prediction of the Microhardness Characteristics, the Removable Material Volume for the Durability Period, Cutting Tools Durability and Processing Productivity Depending on the Grain Size of the Coating or Cutting Tool Base Material Measurement and Analysis of Plasma Arc Cutting Acoustic Signal Influence of Pulverized Material on Vibration and Sound Characteristics of an Operating Ball Mill Similitude analysis of free vibration of functionally graded material cylinders under thermal environment Experimental Study on Coupling Characteristics of Cutting Heat and Cutting Vibration Under Different Tool Wear States Building of Ultrasonic Vibration Precision Cutting System and Experimental Study of Cutting for Plastic Material Application of multi-base fusion generalized chirplet basis transform in vibration signal analysis of multiple rotor rotating machinery Free Vibration Characteristics of Multi-Material Lattice Structures Planetary Gearbox Vibration Signal Characteristics Analysis and Fault Diagnosis |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |