Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Effect of Top Sheet Materials on Joint Performance of Self-Piercing Riveting |
Md Abdul Karim, Siva Prasad Murugan, KiMan Bae, Jongjin Baek, Changwook Ji, Wooram Noh, Han-Ju Lee, Will Jang, Duck Bong Kim, Yeong-Do Park |
J Weld Join. 2022;40(6):512-524. Published online 2022 December 30 DOI: https://doi.org/10.5781/JWJ.2022.40.6.7 |
Effect of Top Sheet Materials on Joint Performance of Self-Piercing Riveting Strength modeling of Al-alloy sheet self-piercing riveting considering different failure modes Durability on alternate immersion test of self-piercing riveting aluminium joint A Performance Study of Self-Piercing Riveting of Aluminum and Copper Alloy Sheets Friction Characterisation for a Tumbling Self-Piercing Riveting Process Influence of aluminium sheet surface modification on the self-piercing riveting process and the joint static lap shear strength A Performance Study on Self-Piercing Riveting and Adhesive Hybrid Joints of Different Adhesive Process modeling, joint-property characterization and construction of joint connectors for mechanical fastening by self-piercing riveting Performance of dissimilar metal Self-Piercing Riveting (SPR) joint and coating behaviour under corrosive environment Self-piercing riveting of aluminium–lithium alloy sheet materials |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |