Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Study of Convolution Neural Network Based Deep Learning to Classify the Quality of Self-Piercing Riveting Joint |
Min Gyu Kim, Tae Hyun Lee, Seung Hwan Lee, Cheol Hee Kim, Dong Hyuck Kam |
J Weld Join. 2022;40(6):502-511. Published online 2022 December 30 DOI: https://doi.org/10.5781/JWJ.2022.40.6.6 |
Study of Convolution Neural Network Based Deep Learning to Classify the Quality of Self-Piercing Riveting Joint Crack Detection and Evaluation Method for Self-Piercing Riveting Button Images Based on BP Neural Network Self-piercing riveting process: Prediction of joint characteristics through finite element and neural network modeling An Improved Performance of Deep Learning Based on Convolution Neural Network to Classify the Hand Motion by Evaluating Hyper Parameter A Comparative Study of Self-Piercing Riveting and Friction Self-Piercing Riveting of Cast Aluminum Alloy Al–Si7Mg Dementia detection using the deep convolution neural network method Deep Learning Based Underwater Image Enhancement Using Deep Convolution Neural Network 2022 Second International Conference on Advances in Electrical, Computing, Communication and Sustainable Technologies (ICAECT). 2022; Deep-Learning-Based Predictive Architectures for Self-Piercing Riveting Process Parametric Study of Self-Piercing Riveting for CFRP-Aluminum Dissimilar Joint DCT-based Fast Spectral Convolution for Deep Convolutional Neural Networks |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |