Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Study on Laser Welding of Dissimilar Materials between Aluminum and Copper (Ⅰ) - Research Trend in Laser Welding Technology and Materials Testing Methods -
Yong Kim, Su Jin Jeong, Seong Min Yun, Je In Lee
J Weld Join. 2022;40(5):416-437.   Published online 2022 September 29    DOI: https://doi.org/10.5781/JWJ.2022.40.5.7

Excel Download

Study on Laser Welding of Dissimilar Materials between Aluminum and Copper (Ⅰ) - Research Trend in Laser Welding Technology and Materials Testing Methods -
Journal of Welding and Joining. 2022;40(5):416-437   Crossref logo
Link1 Link2 Link3

A review on dissimilar laser welding of steel-copper, steel-aluminum, aluminum-copper, and steel-nickel for electric vehicle battery manufacturing
Optics & Laser Technology. 2022;146:107595   Crossref logo
Link1 Link2

Laser welding and brazing of dissimilar materials
Handbook of Laser Welding Technologies. 2013;255-279   Crossref logo
Link1 Link2 Link3

A Parametric Study on Dissimilar Metal Welding of Aluminum and Copper using Pulsed Fiber Laser
. 2021;   Crossref logo
Link1 Link2

Research Trend of Laser Welding and Weldability of High Speed Dissimilar Laser Lap Welding for Titanium
Journal of Welding and Joining. 2017;35(4):16-22   Crossref logo
Link1 Link2 Link3

Laser Welding of Thin Copper and Aluminum Sheets: Feasibility and Challenges in Continuous-Wave Welding of Dissimilar Metals
Lasers in Manufacturing and Materials Processing. 2019;6(2):136-157   Crossref logo
Link1 Link2 Link3

The Study on Mechanical Strength of Titanium-Aluminum Dissimilar Butt Joints by Laser Welding-Brazing Process
Materials. 2019;12(5):712   Crossref logo
Link1

Dissimilar Metal Laser Beam Welding Between Aluminum and Copper
Proceedings of the 38th International MATADOR Conference. 2022;763-772   Crossref logo
Link1

Laser Welding, Joining, or Brazing of Dissimilar Materials
Topics in Mining, Metallurgy and Materials Engineering. 2020;167-184   Crossref logo
Link1

Laser Micro Welding of Dissimilar Material of Aluminum and Copper Alloys
Materials Science Forum. 2017;882:18-22   Crossref logo
Link1