Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
A Study on the Microstructure and Mechanical Properties of the Coarse Grain Heat Affected Zone in EH40 Grade High Strength Structural Steels
Seonghoon Jeong, Seunglae Hong, JunSeok Seo, Ji-Hee Son, Hyung Goun Joo
J Weld Join. 2022;40(5):410-415.   Published online 2022 September 29    DOI: https://doi.org/10.5781/JWJ.2022.40.5.6

Excel Download

A Study on the Microstructure and Mechanical Properties of the Coarse Grain Heat Affected Zone in EH40 Grade High Strength Structural Steels
Journal of Welding and Joining. 2022;40(5):410-415   Crossref logo
Link1 Link2 Link3

Effects of Nb on microstructure and continuous cooling transformation of coarse grain heat-affected zone in 610MPa class high-strength low-alloy structural steels
Materials Science and Engineering: A. 2009;499(1-2):182-186   Crossref logo
Link1 Link2

Effect of Niobium Content on the Microstructure and Mechanical Properties of Simulated Coarse-Grained Heat-Affected Zone (CGHAZ) of High-Strength Low-Alloy (HSLA) Steels
Materials. 2022;15(9):3318   Crossref logo
Link1

Influence of Ni and Mn on Microstructure and Mechanical Properties of Coarse Grain Heat Affected Zone in Low Carbon Microalloyed Steel
Energy Materials 2014. 2014;629-637   Crossref logo
Link1

Crystallographic study on microstructure and impact toughness of coarse grained heat affected zone of ultra-high strength steel
Materials Letters. 2022;323:132552   Crossref logo
Link1 Link2

Effect of Welding Heat Input on Microstructure and Properties of Coarse Grain Zone in Heat Affected Zone of Ultra-Low Carbon Bainitic Steel
Materials Research. 2022;25:   Crossref logo
Link1

Effect of Secondary Welding Thermal Cycle Peak Temperature on Microstructure and Properties in Simulated Reheat Coarse Grain Heat Affected Zone of High Strength Medium-Mn Steel
Journal of Materials Engineering and Performance. 2022;   Crossref logo
Link1 Link2 Link3

Grain refinement in the coarse-grained region of the heat-affected zone in low-carbon high-strength microalloyed steels
International Journal of Minerals, Metallurgy, and Materials. 2010;17(6):737-741   Crossref logo
Link1 Link2 Link3

Effect of Cr Content on Microstructure and Impact Toughness in the Simulated Coarse-Grained Heat-Affected Zone of High-Strength Low-Alloy Steels
steel research international. 2016;87(11):1426-1434   Crossref logo
Link1 Link2

Austenite Grain Size Model for the Coarse Grain Heat Affected Zone in Line Pipe Steels
Volume 3: Operations, Monitoring, and Maintenance; Materials and Joining. 2020;   Crossref logo