Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Energy-based Beta Peak Extraction from Dynamic Resistance Curves
JaHun Ku, Youngdo Park, Namkug Ku
J Weld Join. 2022;40(5):401-409.   Published online 2022 September 29    DOI: https://doi.org/10.5781/JWJ.2022.40.5.5

Excel Download

Energy-based Beta Peak Extraction from Dynamic Resistance Curves
Journal of Welding and Joining. 2022;40(5):401-409   Crossref logo
Link1 Link2 Link3

Logistic curves, extraction costs and effective peak oil
Energy Policy. 2012;51:586-597   Crossref logo
Link1 Link2

Dynamic liquid level prediction in oil wells during oil extraction based on WOA-AM-LSTM-ANN model using dynamic and static information
Energy. 2023;282:128981   Crossref logo
Link1 Link2

96/04953 Role of dynamic properties of bitumen extraction from Athabasca oil sands
Fuel and Energy Abstracts. 1996;37(5):349   Crossref logo
Link1 Link2

Model-based dynamic multi-parameter method for peak power estimation of lithium–ion batteries
Applied Energy. 2012;96:378-386   Crossref logo
Link1 Link2

Peak regulation performance study of the gas turbine combined cycle based combined heating and power system with gas turbine interstage extraction gas method
Energy Conversion and Management. 2022;269:116103   Crossref logo
Link1 Link2

Improved extraction of I–V curves from low-energy electron diffraction images
Chemical Physics Letters. 2012;532:116-118   Crossref logo
Link1 Link2

High performing extraction procedure for the one-diode model of a photovoltaic panel from experimental I–V curves by using reduced forms
Solar Energy. 2014;103:316-326   Crossref logo
Link1 Link2

Prices vs. quantities in a dynamic problem: Externalities from resource extraction
Resource and Energy Economics. 2011;33(4):843-854   Crossref logo
Link1 Link2

Combustion Optimization Under Deep Peak Shaving Based on DYNA-A3C With Dynamic Weight
Frontiers in Energy Research. 2023;10:   Crossref logo
Link1