Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Heat Treatment Conditions on Resistance Spot Weldability of 1.8 GPa-grade Al-Si Coated Hot Stamping Boron Steel
Jaehun Kim, Hyunuk Jun, Wonho Kim, Jooyong Cheon, Jaedeuk Kim, Ilguk Jo, Changwook Ji
J Weld Join. 2022;40(4):311-321.   Published online 2022 August 31    DOI: https://doi.org/10.5781/JWJ.2022.40.4.3

Excel Download

Effect of Heat Treatment Conditions on Resistance Spot Weldability of 1.8 GPa-grade Al-Si Coated Hot Stamping Boron Steel
Journal of Welding and Joining. 2022;40(4):311-321   Crossref logo
Link1 Link2 Link3

A Study on Laser Weldability of Al-Si Coated Boron Steel According to Hot-Stamping Heat Treatment
Advanced Materials Research. 2015;1110:113-117   Crossref logo
Link1

Effect of Hot Stamping Heat Treatment Temperature on Resistance Spot Weldability of Al-10% Si Coated 30MnB5 Steel
Korean Journal of Metals and Materials. 2019;57(12):778-786   Crossref logo
Link1 Link2 Link3

Effect of heat treatment on weldability of Al Si coated hot-stamped Usibor® 1500P
Surface and Coatings Technology. 2022;445:128750   Crossref logo
Link1 Link2

Trend of Resistance Spot Welding Technology of Al-Si Coated Hot-Stamped Boron Steel for Automobile Body
Journal of Welding and Joining. 2022;40(2):187-197   Crossref logo
Link1 Link2 Link3

Laser welding of Al-Si coated hot stamping steel
Procedia Engineering. 2011;10:2226-2231   Crossref logo
Link1 Link2

Effect of Heat Treatment on the Formability of Zn‐Coated Hot Stamping Steel
steel research international. 2022;93(7):2100725   Crossref logo
Link1 Link2 Link3

Effect of Part/Die Boundary Conditions on Microstructural Evolution during Hot Stamping 2000 MPa Class Boron Steel
steel research international. 2018;89(6):1700495   Crossref logo
Link1 Link2

Effects of Al-Si Coating on Static and Dynamic Strength of Spot-Welded Hot-Stamping Steel Joints
Metals. 2021;11(6):976   Crossref logo
Link1

Recent Trends to Improve Laser Weldability of Al-Si coated Hot-stamped Boron Steel
Journal of Welding and Joining. 2022;40(2):175-186   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.