CrossRef Text and Data Mining |
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Effect of Additive Machines and Powders on Mechanical Properties of Stainless Steel 316L Manufactured by L-PBF |
Dongjin Oh, Youngjun Kang, Kidong Kim |
J Weld Join. 2022;40(4):322-328. Published online 2022 August 31 DOI: https://doi.org/10.5781/JWJ.2022.40.4.4 |
Effect of Additive Machines and Powders on Mechanical Properties of Stainless Steel 316L Manufactured by L-PBF Effect of High Laser Energy Density on Selective Laser Melted 316L Stainless Steel: Analysis on Metallurgical and Mechanical Properties and Comparison with Wrought 316L Stainless Steel Effect of Processing Atmosphere and Secondary Operations on the Mechanical Properties of Additive Manufactured AISI 316L Stainless Steel by Plasma Metal Deposition Mechanical Properties of 3-D LENS and PBF Printed Stainless Steel 316L Prototypes Comparison of Polishing Methods: The Effect on The Surface Roughness and Fatigue Performance of PBF-LB manufactured 316L Stainless Steel 2022 7th National Scientific Conference on Applying New Technology in Green Buildings (ATiGB). 2022; Mechanical properties and microstructure evolution of additive manufactured 316L stainless steel under dynamic loading Particle Erosion Performance of Additive Manufactured 316L Stainless Steel Materials Size-dependent stochastic tensile properties in additively manufactured 316L stainless steel High-throughput surface characterization to identify porosity defects in additively manufactured 316L stainless steel Effect of post process shear straining on structure and mechanical properties of 316 L stainless steel manufactured via powder bed fusion |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |