Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Metallurgical Factors Affecting the Tensile Properties of Weld Heat-Affected Zone in Medium Mn Transformation-Induced Plasticity Steel
Gitae Park
J Weld Join. 2022;40(4):329-336.   Published online 2022 August 18    DOI: https://doi.org/10.5781/JWJ.2022.40.4.5

Excel Download

Metallurgical Factors Affecting the Tensile Properties of Weld Heat-Affected Zone in Medium Mn Transformation-Induced Plasticity Steel
Journal of Welding and Joining. 2022;40(4):329-336   Crossref logo
Link1 Link2 Link3

Effects of in-situ post-weld heat treatment on the microstructure and mechanical properties of the coarse-grained heat-affected zone in a resistance spot weld in medium Mn TRIP steel
Materials Science and Engineering: A. 2020;788:139477   Crossref logo
Link1 Link2

On Factors Affecting the Phase Transformation and Mechanical Properties of Cold-Rolled Transformation-Induced-Plasticity–Aided Steel
Metallurgical and Materials Transactions A. 2008;39(10):2513-2527   Crossref logo
Link1 Link2 Link3

Enhanced Impact Toughness of Heat Affected Zone in Gas Shield Arc Weld Joint of Low‐C Medium‐Mn High Strength Steel by Post‐Weld Heat Treatment
steel research international. 2017;89(4):1700422   Crossref logo
Link1 Link2 Link3 Link4

Tensile Deformation Behavior and Phase Transformation in the Weld Coarse-Grained Heat-Affected Zone of Metastable High-Nitrogen Fe-18Cr-10Mn-N Stainless Steel
Metallurgical and Materials Transactions A. 2013;44(7):3069-3076   Crossref logo
Link1 Link2 Link3

Dynamic Tensile Behavior of Fiber Laser Welds of Medium Manganese Transformation-Induced Plasticity Steel
Metallurgical and Materials Transactions A. 2019;50(8):3578-3588   Crossref logo
Link1 Link2 Link3

Impact Toughness of Medium-Mn Transformation-Induced Plasticity-Aided Steels
steel research international. 2015;86(10):1151-1160   Crossref logo
Link1 Link2

Continuous cooling transformation diagram and mechanical properties in weld coarse-grain heat-affected zone of API X70 steel
Sādhanā. 2021;46(2):   Crossref logo
Link1 Link2 Link3

Simultaneous Increase of Both Strength and Ductility of Medium Mn Transformation-Induced Plasticity Steel by Vanadium Alloying
Metallurgical and Materials Transactions A. 2018;49(5):1433-1438   Crossref logo
Link1 Link2 Link3

Microstructure and Local Mechanical Properties of the Heat-Affected Zone of a Resistance Spot Welded Medium-Mn Steel
Materials. 2021;14(12):3362   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.