Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Effect of Line-Heating on the Microstructural and Mechanical Characteristics of 320-MPa-Grade High-Strength Hull Plates |
Seonghoon Jeong, Seunglae Hong, JunSeok Seo, Woohyuk Choi |
J Weld Join. 2022;40(4):352-357. Published online 2022 July 20 DOI: https://doi.org/10.5781/JWJ.2022.40.4.8 |
Effect of Line-Heating on the Microstructural and Mechanical Characteristics of 320-MPa-Grade High-Strength Hull Plates Effect of welding processes on mechanical and microstructural characteristics of high strength low alloy naval grade steel joints Effect of Nitrogen Content and Cooling Rate on Transformation Characteristics and Mechanical Properties for 600 MPa High Strength Rebar The effect of CO2 laser cutting parameter on Mechanical & Microstructural characteristics of high strength steel-a review Effect of martensite fine structure on mechanical properties of an 1100 MPa grade ultra-high strength steel Strength and deformability of welded joints of 780 MPa grade steel plates Mechanical Clinching and Self-Pierce Riveting of Thin Three Sheets of 5000 Series Aluminium Alloy and 980 MPa Grade Cold Rolled Ultra-High Strength Steel Microstructural Characterization and Mechanical Properties of Electron Beam Welded Joint of High Strength Steel Grade S690QL Effect of Inclusions and Microstructural Characteristics on the Mechanical Properties and Fracture Behavior of a High- Strength Low- Alloy Steel Development of high-formability high-strength galvannealed steel sheet of tensile strength 440 MPa grade with excellent formability |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |