Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
A Review of the Brazeability of Low-Temperature and Nano-Reinforced Al-Based Brazing Filler Metals |
Furkan, Hye-Jeong Kim, Gun-hwan Lee, Jae Pil Jung |
J Weld Join. 2022;40(3):216-224. Published online 2022 June 17 DOI: https://doi.org/10.5781/JWJ.2022.40.3.2 |
A Review of the Brazeability of Low-Temperature and Nano-Reinforced Al-Based Brazing Filler Metals Influence of Nanosized AlN Powders on the Microstructure, Brazeability, and Tensile Properties of Al-based Filler for Low Temperature Al/Cu Dissimilar Brazing High-temperature brazing: filler metals and processing Vacuum Brazing of 55 vol.% SiCp/ZL102 Composites Using Micro-Nano Brazing Filler Metal Fabricated by Melt-Spinning Brazing of nickel-based filler metals for pipes and other components in contact with drinking water Low-Temperature Brazing of Titanium Using Al-Based Filler Alloys Fatigue and Creep Properties of Al-Si Brazing Filler Metals Research and Development of Powder Brazing Filler Metals for Diamond Tools: A Review High-Temperature Brazing of Superalloys and Stainless Steels with Novel Ductile Ni-Hf-Based Filler Metals Effect of ZrO2 Nanomaterials on Wettability and Interfacial Characteristics of Al-19Cu-11Si-2Sn Filler Metal for Low Temperature Al to Cu Dissimilar Brazing |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |