Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Study of the Change in Surface Wettability for Zircaloy-4 Utilizing Spatially Homogenized Nanosecond Laser Beam
Daewong Park, Sungyoon Lee, Seungjin Hwang, Geonhui Lee, Hanjin Jo, Sanghyun Park, Seryeyohan Cho, Tae Jun Yu
JWJ. 2022;40(2):156-164.   Published online 2022 April 15    DOI: https://doi.org/10.5781/JWJ.2022.40.2.7

Excel Download

Study of the Change in Surface Wettability for Zircaloy-4 Utilizing Spatially Homogenized Nanosecond Laser Beam
Journal of Welding and Joining. 2022;40(2):156-164   Crossref logo
Link1 Link2 Link3

TiN growth on Si(100) by pulsed laser deposition using homogenized KrF excimer laser beam
Applied Surface Science. 1999;138-139:335-339   Crossref logo
Link1 Link2

A Comparative Study on the Wettability of Unstructured and Structured LiFePO4 with Nanosecond Pulsed Fiber Laser
Micromachines. 2021;12(5):582   Crossref logo
Link1

Wettability and friction control of a stainless steel surface by combining nanosecond laser texturing and adsorption of superhydrophobic nanosilica particles
Scientific Reports. 2018;8(1):   Crossref logo
Link1 Link2 Link3

Nanosecond laser surface modification of AISI 304L stainless steel: Influence the beam overlap on pitting corrosion resistance
Applied Surface Science. 2014;288:34-39   Crossref logo
Link1 Link2

Wavelength dependant ablation rates for metals and silicate glasses using homogenized laser beam profiles — implications for LA-ICP-MS
Applied Surface Science. 2001;182(1-2):91-102   Crossref logo
Link1 Link2

Impact of yttrium ion implantation on corrosion behavior of laser beam welded zircaloy-4 in sulfuric acid solution
Applied Surface Science. 2005;252(5):1974-1980   Crossref logo
Link1 Link2

Switchable wettability control of titanium via facile nanosecond laser-based surface texturing
Surfaces and Interfaces. 2021;24:101122   Crossref logo
Link1 Link2

Leidenfrost Effect and Surface Wettability
The Surface Wettability Effect on Phase Change. 2022;189-233   Crossref logo
Link1

Hybrid atomistic-macroscale modeling of long-time phase change in nanosecond laser–material interaction
Applied Surface Science. 2008;255(5):3097-3103   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.