Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Recrystallization Behavior of CP Ti Welds by Rolling
Byoung-Hyun Yoon, Ji-Yeon Shim, Bong-Yong Kang
JWJ. 2021;39(6):577-581.   Published online 2021 December 9    DOI: https://doi.org/10.5781/JWJ.2021.39.6.1

Excel Download

Recrystallization Behavior of CP Ti Welds by Rolling
Journal of Welding and Joining. 2021;39(6):577-581   Crossref logo
Link1 Link2 Link3

Recrystallization and precipitation behavior of low-activation V–Cr–Ti alloys after cold rolling
Journal of Nuclear Materials. 2004;325(1):53-60   Crossref logo
Link1 Link2

Influence of α Region Hot Rolling on the Rolling and Recrystallization Texture of Cold Rolled Ti-Bearing Extra Low Carbon Steel Sheets
Materials Science Forum. 1994;157-162:1051-1056   Crossref logo
Link1

Crystal Plasticity modeling of dynamic recrystallization in CP Ti
Procedia Structural Integrity. 2019;14:251-258   Crossref logo
Link1 Link2

The Effect of Nb-Ti on Cold Rolling Texture and Recrystallization Texture of B4003M
Advanced Materials Research. 2011;181-182:1054-1058   Crossref logo
Link1

Strengthening of CP-Ti by Rolling at Room Temperature
Materials Science Forum. 2010;667-669:737-741   Crossref logo
Link1

Texture evolution during cold rolling and recrystallization of L12-type ordered Ni3(Si,Ti) alloy
Intermetallics. 2002;10(7):693-700   Crossref logo
Link1 Link2

Texture Evolution Behavior and Its Triggered Mechanical Anisotropy of CP Ti During Severe Cold Rolling and Subsequent Annealing
Acta Metallurgica Sinica (English Letters). 2020;33(9):1271-1282   Crossref logo
Link1 Link2 Link3

Microstructural and microtextural analysis of InterPulse GTCAW welds in Cp-Ti and Ti–6Al–4V
Materials Science and Engineering: A. 2010;527(29-30):7694-7705   Crossref logo
Link1 Link2

Recrystallization Behavior of Aluminum Layers in Al/Ti/Si and Al/Ti/SiOx/Si Structures
Inorganic Materials. 2005;41(8):807-811   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.