CrossRef Text and Data Mining
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Study on the Microstructure and Mechanical Properties of Butt GMAW Al/Fe Dissimilar Joints using Pure Copper Filler Metal
Ju-Hee Jung, Dae-Woong Park, Eung-Ryul Baek
JWJ. 2021;39(6):641-648.   Published online 2021 December 9    DOI: https://doi.org/10.5781/JWJ.2021.39.6.9

Excel Download

Study on the Microstructure and Mechanical Properties of Butt GMAW Al/Fe Dissimilar Joints using Pure Copper Filler Metal
Journal of Welding and Joining. 2021;39(6):641-648   Crossref logo
Link1 Link2 Link3

Experimental Study on Micro-Friction Stir Welding of Dissimilar Butt Joints Between Al 1050 and Pure Copper
Metallography, Microstructure, and Analysis. 2021;10(4):458-473   Crossref logo
Link1 Link2 Link3

A Study of Filler Metal Effecting on Mechanical Properties for Dissimilar Gas Metal Arc Welding (GMAW) for Austenitic Stainless Steel
Advanced Materials Research. 2013;647:692-696   Crossref logo
Link1

Microstructure and mechanical properties of dissimilar pure copper/1350 aluminum alloy butt joints by friction stir welding
Transactions of Nonferrous Metals Society of China. 2012;22(6):1298-1306   Crossref logo
Link1 Link2

Microstructure and mechanical properties of gas metal arc welded AISI 430/AISI 304 dissimilar stainless steels butt joints
Journal of Physics: Conference Series. 2021;1777(1):012047   Crossref logo
Link1 Link2 Link3 Link4

Microstructure and Properties of Mg/Al Dissimilar Joints by GTAW with Al-Si Filler Wire
Advanced Materials Research. 2014;941-944:2035-2038   Crossref logo
Link1

Microstructure & mechanical properties of dissimilar material joints between T91 martensitic & S304H austenitic steels using different filler wires
Materials Today: Proceedings. 2021;46:9397-9404   Crossref logo
Link1 Link2

Microstructure evolution of Al/Mg butt joints welded by gas tungsten arc with Zn filler metal
Materials Characterization. 2012;69:84-89   Crossref logo
Link1 Link2

Effect of Al foils interlayer on microstructures and mechanical properties of Mg–Al butt joints welded by gas tungsten arc welding filling with Zn filler metal
Materials & Design. 2013;46:419-425   Crossref logo
Link1 Link2

Microstructure and mechanical properties of dissimilar pure copper foil/1050 aluminium composites made with composite metal foil manufacturing
Journal of Materials Processing Technology. 2016;238:96-107   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.