Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Dimension Precision and Uniformability Depending on the Interpass Distance Variation of Automated-Wire Arc Additive Manufacturing using 5 Cr-4 Mo Tool Steel Alloy
Jae-Deuk Kim, Jae Won Kim, Joo Yong Cheon, Sungwook Kang, Yeong-Do Park, Changwook Ji
JWJ. 2021;39(6):613-624.   Published online 2021 December 6    DOI: https://doi.org/10.5781/JWJ.2021.39.6.6

Excel Download

Dimension Precision and Uniformability Depending on the Interpass Distance Variation of Automated-Wire Arc Additive Manufacturing using 5 Cr-4 Mo Tool Steel Alloy
Journal of Welding and Joining. 2021;39(6):613-624   Crossref logo
Link1 Link2 Link3

Dissimilar metal deposition with a stainless steel and nickel-based alloy using wire and arc-based additive manufacturing
Precision Engineering. 2016;45:387-395   Crossref logo
Link1 Link2

3D printing in steel construction with the automated Wire Arc Additive Manufacturing
Steel Construction. 2019;12(2):104-104   Crossref logo
Link1 Link2

Effects of Interpass Cooling on Material Properties of Wire Arc Additive Manufactured Al–6.3Mg Alloy
3D Printing and Additive Manufacturing. 2019;6(6):344-353   Crossref logo
Link1 Link2

Prediction of the interpass temperature of a wire arc additive manufactured wall: FEM simulations and artificial neural network
Additive Manufacturing. 2021;48:102387   Crossref logo
Link1 Link2

Influence of Interpass Temperature on Wire Arc Additive Manufacturing (WAAM) of Aluminium Alloy Components
MATEC Web of Conferences. 2019;269:05001   Crossref logo
Link1

Deformation Behavior of a High-Entropy Al–Co–Cr–Fe–Ni Alloy Fabricated by Means of Wire-Arc Additive Manufacturing
Steel in Translation. 2021;51(1):27-32   Crossref logo
Link1 Link2 Link3

Effect of Filler Metal Type on Microstructure and Mechanical Properties of Fabricated NiAl Bronze Alloy Using Wire Arc Additive Manufacturing System
Metals. 2021;11(3):513   Crossref logo
Link1

Continuous Eulerian tool path strategies for wire-arc additive manufacturing of rib-web structures with machine-learning-based adaptive void filling
Additive Manufacturing. 2020;35:101265   Crossref logo
Link1 Link2

Wire arc additive manufacturing: approaches and future prospects
Additive Manufacturing. 2021;183-208   Crossref logo