Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Property Evaluation and Fabrication of WC-Co-Si3N4 Hard Materials by a Rapid Sintering Process
Jeong-Han Lee, Hyun-Kuk Park
JWJ. 2021;39(6):625-631.   Published online 2021 December 6    DOI: https://doi.org/10.5781/JWJ.2021.39.6.7

Excel Download

Hybrid Microwave-Assisted Rapid Sintering Process for Fabrication of Sn-0.7Cu+1.0wt.%Si3N4 Composite Solder
Materials Science Forum. 2014;803:305-309   Crossref logo
Link1

Effect of DC Pulse Patterns on Spark Plasma Sintering Process of [Fe0.8Co0.2B0.05Si0.2]96Nb4 Bulk Metallic Glass
Materials Science Forum. 2016;849:28-33   Crossref logo
Link1

Gas Pressure Sintering of Si3N4 in N2/CO/(CO2) Atmosphere
Key Engineering Materials. 1993;89-91:187-192   Crossref logo
Link1

Fabrication Process and Properties of Si3N4-SiC Ceramics by a Two Step Sintering Method
Advanced Materials Research. 2012;476-478:570-573   Crossref logo
Link1

Effect of Sintering Process on Fabrication of Porous Si3N4/SiC Composites
Key Engineering Materials. 2007;353-358:1572-1575   Crossref logo
Link1

Rapid Sintering of Nanostructural Powder to Form Si3N4
Materials Science Forum. 1998;269-272:219-226   Crossref logo
Link1

Investigation of Microstructure and Property of the Fe3Al/Al2O3 Composites Fabricated by Mechanical Alloying Process and Plasma Active Sintering Process
Advanced Materials Research. 2011;194-196:1689-1692   Crossref logo
Link1

Investigation of Fabrication and Microstructure of the Fe3Al/Al2O3 Composites by Plasma Active Sintering Process
Advanced Materials Research. 2010;160-162:1458-1463   Crossref logo
Link1

Effect of Sintering Temperature on the Oxygen Adsorption Property of Ba0.8Sr0.2Fe0.5Co0.5O3-δ
Advanced Materials Research. 2013;710:72-75   Crossref logo
Link1

Nucleation and Growth of Si2N2O in Si3N4-Materials Employing Different Sintering Additives
Key Engineering Materials. 1993;89-91:483-488   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.