Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effects of High-Power Laser Heat Input on the Mechanical Properties of GPa-Grade Advanced High Strength TRIP Steel
Sangwoo Nam, Hyung Won Lee, Cheolhee Kim, Chul-Young Jung, Yonung-Min KIm
J Weld Join. 2021;39(5):505-512.   Published online 2021 October 20    DOI: https://doi.org/10.5781/JWJ.2021.39.5.6

Excel Download

Effects of High-Power Laser Heat Input on the Mechanical Properties of GPa-Grade Advanced High Strength TRIP Steel
Journal of Welding and Joining. 2021;39(5):505-512   Crossref logo
Link1 Link2 Link3

Effects of Retained Austenite Stability on Mechanical Properties of High Strength TRIP Steel
Advanced Materials Research. 2012;602-604:287-293   Crossref logo
Link1

Microstructure and Mechanical Properties of High Strength Hot-Rolled TRIP Steel Containing Vanadium
Advanced Materials Research. 2010;160-162:324-329   Crossref logo
Link1

Structure and Mechanical Properties of High-Strength Austenitic-Martensitic Trip-Steel VNS9-Sh
Metal Science and Heat Treatment. 2019;61(1-2):10-14   Crossref logo
Link1 Link2 Link3

A Novel Low-Carbon High-Strength Steel: Processing, Microstructure and Mechanical Properties
Advanced High Strength Steel. 2018;125-133   Crossref logo
Link1

Metallurgical and mechanical properties of laser welded high strength low alloy steel
Journal of Advanced Research. 2016;7(3):463-472   Crossref logo
Link1 Link2

Effects of Different Types of Steel Fibers on the Mechanical Properties of High Strength Concrete
Advanced Materials Research. 2014;1054:80-84   Crossref logo
Link1

Effect of Heat Treatment on Mechanical Properties of 1500MPa High Strength Wear-Resistant Steel
Advanced Materials Research. 2010;168-170:847-851   Crossref logo
Link1

Effects of Welding Positions on Mechanical Properties and Microstructure in Weld Metal of High Strength Steel
Advanced Materials Research. 2009;83-86:1121-1127   Crossref logo
Link1

Heat treatment and heat input effects on the dissimilar laser beam welded AISI 904L super austenitic stainless steel to AISI 317L austenitic stainless steel: Surface, texture, microstructure and mechanical properties
Vacuum. 2022;205:111440   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.