Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Effect of Decomposed Microstructure on Mechanical Properties of Additively Manufactured Ti-6Al-4V Alloy
Desrilia Nursyifaulkhair, Nokeun Park, Eung Ryul Baek
JWJ. 2021;39(5):527-535.   Published online 2021 September 17    DOI: https://doi.org/10.5781/JWJ.2021.39.5.9

Excel Download

The Effect of Decomposed Microstructure on Mechanical Properties of Additively Manufactured Ti-6Al-4V Alloy
Journal of Welding and Joining. 2021;39(5):527-535   Crossref logo
Link1 Link2 Link3

Improvement of microstructure and mechanical properties in Wire + Arc Additively Manufactured Ti-6Al-4V with Machine Hammer Peening
Procedia Engineering. 2017;216:8-17   Crossref logo
Link1 Link2

Effect of Transverse Magnetic Field On Microstructure And Mechanical Properties of Ti-6Al-4V Manufactured By Laser-MIG Hybrid Welding
. 2021;   Crossref logo
Link1 Link2

Modeling of Processing-Induced Pore Morphology in an Additively-Manufactured Ti-6Al-4V Alloy
Materials. 2017;10(2):145   Crossref logo
Link1

Effect of Hydrogenation on Microstructure and Mechanical Properties of Ti-6Al-4V Titanium Alloy
Advanced Materials Research. 2013;750-752:596-602   Crossref logo
Link1

Microstructure and Mechanical Properties of Ti-6Al-4V Manufactured by SLM
Key Engineering Materials. 2015;651-653:677-682   Crossref logo
Link1

In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance
Acta Materialia. 2017;125:390-400   Crossref logo
Link1 Link2

Microstructure and Mechanical Properties of Wrought and Additive Manufactured Ti-6Al-4V Cylindrical Bars
Procedia Technology. 2015;20:231-236   Crossref logo
Link1 Link2

Microstructure and Mechanical Properties of Carbon/Carbon Composites Infiltrated with Ti–6Al–4V Titanium Alloy
Crystals. 2020;10(1):29   Crossref logo
Link1

Fatigue Property of Additively Manufactured Ti-6Al-4V under Non-proportional Multiaxial Loading
. 2021;   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.