Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Evaluation of Weldability based on Alignment Condition of Horns and Anvils used in Multilayered Battery Cell Welding Process in Ultrasonic Metal Welding
Seungmin Shin, Dongcheol Kim
JWJ. 2021;39(5):552-557.   Published online 2021 September 15    DOI: https://doi.org/10.5781/JWJ.2021.39.5.12

Excel Download

Evaluation of Weldability based on Alignment Condition of Horns and Anvils used in Multilayered Battery Cell Welding Process in Ultrasonic Metal Welding
Journal of Welding and Joining. 2021;39(5):552-557   Crossref logo
Link1 Link2 Link3

Studies on thermo-elastic heating of horns used in ultrasonic plastic welding
Ultrasonics. 2015;55:123-132   Crossref logo
Link1 Link2

Ultrasonic Metal Welding of Multilayered Copper Foils to Nickel-Plated Copper Sheet in Lithium-Ion Battery Cell
Metals. 2021;11(8):1195   Crossref logo
Link1

Ultrasonic metal welding
New Developments in Advanced Welding. 2005;241-269   Crossref logo
Link1 Link2 Link3

Weldability appraisement of dissimilar metal joints: application of ultrasonic spot welding to Li-ion batteries
Modern Manufacturing Processes. 2020;43-68   Crossref logo
Link1 Link2

High power resonant horns for ultrasonic welding and their material aspects
Ultrasonics. 1987;25(6):371   Crossref logo
Link1 Link2

Designing of Ultrasonic Horns to Improve Amplitude Uniformity in Ultrasonic Metal Welding
MATEC Web of Conferences. 2019;257:02009   Crossref logo
Link1

Single-shot explosive welding technique for the fabrication of multilayered metal base composites: effect of welding parameters leading to optimum bonding condition
Composites Engineering. 1995;5(8):1069-1079   Crossref logo
Link1 Link2

Weldability Evaluation of 409 FSS with A-TIG Welding Process
Materials Today: Proceedings. 2019;18:3052-3060   Crossref logo
Link1 Link2

Ultrasonic and Laser Welding Technologies on Al/Cu Dissimilar Materials for the Lithium-Ion Battery Cell or Module Manufacturing
Journal of Welding and Joining. 2019;37(2):52-59   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.