Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Microstructure on Low-Temperature Impact Toughness of Multi-Pass Weld Metal of 1 GPa Class High Strength Steel
Yongjoon Kang, Changhee Lee
JWJ. 2021;39(3):233-238.   Published online 2021 June 24    DOI: https://doi.org/10.5781/JWJ.2021.39.3.1

Excel Download

Effect of Microstructure on Low-Temperature Impact Toughness of Multi-Pass Weld Metal of 1 GPa Class High Strength Steel
Journal of Welding and Joining. 2021;39(3):233-238   Crossref logo
Link1 Link2 Link3

Correlation Between Microstructure and Low-Temperature Impact Toughness of Simulated Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel
Metallurgical and Materials Transactions A. 2017;49(1):177-186   Crossref logo
Link1 Link2 Link3

Microstructure evolution and impact toughness variation for high strength steel multi-pass weld metals with various cooling rates
Journal of Manufacturing Processes. 2021;65:245-257   Crossref logo
Link1 Link2

Characterization of the Multi-Pass Weld Metal and the Effect of Post-Weld Heat Treatment on Its Microstructure and Toughness
HSLA Steels 2015, Microalloying 2015 & Offshore Engineering Steels 2015. 2016;481-488   Crossref logo
Link1

Nucleation Behavior of Acicular Ferrite in 1 GPa Class High Strength Steel Weld Metal
Journal of Welding and Joining. 2019;37(1):21-26   Crossref logo
Link1 Link2 Link3

Interrelationships between yield strength, low-temperature impact toughness, and microstructure in low-carbon, copper-precipitation-strengthened, high-strength low-alloy plate steels
Materials Science and Engineering: A. 2018;711:424-433   Crossref logo
Link1 Link2

Development of surface coatings for high-strength low alloy steel filler wires and their effect on the weld metal microstructure and properties
Welding in the World. 2021;65(8):1591-1597   Crossref logo
Link1 Link2 Link3

Effect of Microstructure and Segregation of Elements on the Impact Toughness of High-Strength Low-Carbon Bainitic Steel
Metal Science and Heat Treatment. 2016;58(3-4):138-141   Crossref logo
Link1 Link2 Link3

Effect of weld thermal cycle on microstructure and fracture toughness of simulated heat-affected zone for a 800MPa grade high strength low alloy steel
Journal of Materials Processing Technology. 2008;207(1-3):30-39   Crossref logo
Link1 Link2

Influence of welding pass on microstructure and toughness in the reheated zone of multi-pass weld metal of 550 MPa offshore engineering steel
Materials Science and Engineering: A. 2017;702:196-205   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.