CrossRef Text and Data Mining
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Evaluating the Welding Pulses of Various Tool Profiles in Single-Pass Friction Stir Welding of 6082-T6 Aluminium Alloy
S. Gopi, Dhanesh G Mohan
J Weld Join. 2021;39(3):284-294.   Published online 2021 June 8    DOI: https://doi.org/10.5781/JWJ.2021.39.3.7

Excel Download

Evaluating the Welding Pulses of Various Tool Profiles in Single-Pass Friction Stir Welding of 6082-T6 Aluminium Alloy
Journal of Welding and Joining. 2021;39(3):284-294   Crossref logo
Link1 Link2 Link3

Experimental comparison of friction stir welding process and TIG welding process for 6082-T6 Aluminium alloy
Materials Today: Proceedings. 2017;4(2):3590-3600   Crossref logo
Link1 Link2

Influence of tool pin profiles on friction stir welding with a gap for AA6082-T6 aluminium alloy
Materials Research Express. 2019;6(8):086543   Crossref logo
Link1 Link2 Link3 Link4 Link5 Link6 Link7 Link8

Acoustic analysis in friction stir welding of 6082 - T6 aluminium alloy plates
Materials Today: Proceedings. 2019;19:161-169   Crossref logo
Link1 Link2

Friction Stir Welding Tool Design and Their Effect on Welding of AA-6082 T6
Materials Today: Proceedings. 2017;4(8):7962-7970   Crossref logo
Link1 Link2

Welding Repair of Aluminium Alloy 6082 T6 by TIG Welding Process
Materials Science Forum. 2016;872:3-7   Crossref logo
Link1

Multi-Objective Optimization of Friction Stir Welding of Aluminium Alloy 6082-T6 Using hybrid Taguchi-Grey Relation Analysis- ANN Method
Materials Today: Proceedings. 2018;5(2):7150-7159   Crossref logo
Link1 Link2

Effect of Welding Speed on Mechanical Properties of Friction Stir Welded AA 6082-T6 Al Alloy
Applied Mechanics and Materials. 2018;877:98-103   Crossref logo
Link1

Laser beam welding and friction stir welding of 6013-T6 aluminium alloy sheet
Materialwissenschaft und Werkstofftechnik. 2000;31(12):1017-1026   Crossref logo
Link1 Link2

Hybrid Self-Reacting Friction Stir Welding of AA 6061-T6 Aluminium Alloy with Cooling Assisted Approach
Metals. 2020;11(1):16   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.