Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Residual Stress Study of High Manganese Steel Riser Pipe Manufactured by Longitudinal Butt Welding (2) : Equation for Predicting Welding Induced Residual Stresses Established through Parametric Study
Myung-Su Yi, Jung-Kwan Seo
JWJ. 2021;39(2):144-149.   Published online 2021 April 23    DOI: https://doi.org/10.5781/JWJ.2021.39.2.2

Excel Download

Residual Stress Study of High Manganese Steel Riser Pipe Manufactured by Longitudinal Butt Welding (2) : Equation for Predicting Welding Induced Residual Stresses Established through Parametric Study
Journal of Welding and Joining. 2021;39(2):144-149   Crossref logo
Link1 Link2 Link3

Residual Stress Study of High Manganese Steel Riser Pipe Manufactured by Longitudinal Butt Welding (1) : Residual Stress Measurement and FE Analysis
Journal of Welding and Joining. 2021;39(2):135-143   Crossref logo
Link1 Link2 Link3

Neutron Diffraction Investigation of Residual Stresses Induced in Niobium-Steel Bilayer Pipe Manufactured by Explosive Welding
Materials Science Forum. 2013;768-769:697-704   Crossref logo
Link1

RESIDUAL STRESSES AS A CONSEQUENCE OF WELDING
Residual Stresses. 1987;39-58   Crossref logo
Link1 Link2

Prediction of welding residual stress in multi-pass butt-welded modified 9Cr–1Mo steel pipe considering phase transformation effects
Computational Materials Science. 2006;37(3):209-219   Crossref logo
Link1 Link2

Numerical and experimental investigations on welding residual stress in multi-pass butt-welded austenitic stainless steel pipe
Computational Materials Science. 2008;42(2):234-244   Crossref logo
Link1 Link2

A parametric study of thermal and residual stress fields in lined pipe welding
Thermal Science and Engineering Progress. 2017;4:205-218   Crossref logo
Link1 Link2

Measuring welding-induced distortion
Processes and Mechanisms of Welding Residual Stress and Distortion. 2005;209-224   Crossref logo
Link1 Link2 Link3

Study on the Welding Residual Stress in Anchorage Area of Steel Bridge
Advanced Materials Research. 2011;255-260:324-327   Crossref logo
Link1

Numerical simulation of residual stresses induced by laser beam welding in a SUS316 stainless steel pipe with considering initial residual stress influences
Nuclear Engineering and Design. 2010;240(4):688-696   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.