Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
A Study on the Correlation between Bead Geometry and Tensile Strength of Single Lap jointed Dissimilar Combinations through Regression Analysis
Jae Won Kim, Jae-Hwang Kim, Kwang-jin Lee, Sung-Wook Kang, Changwook Ji
JWJ. 2021;39(2):159-166.   Published online 2021 April 20    DOI: https://doi.org/10.5781/JWJ.2021.39.2.4

Excel Download

A Study on the Correlation between Bead Geometry and Tensile Strength of Single Lap jointed Dissimilar Combinations through Regression Analysis
Journal of Welding and Joining. 2021;39(2):159-166   Crossref logo
Link1 Link2 Link3

Single and dual adhesive bond strength analysis of single lap joint between dissimilar adherends
International Journal of Adhesion and Adhesives. 2019;92:142-153   Crossref logo
Link1 Link2

Evaluation of Tensile Shear Strength for Lap Joint of Dissimilar Steels
Materials Science Forum. 2021;1016:1454-1459   Crossref logo
Link1

The effect of opposing notch geometry on the tensile strength of adhesively bonded single-lap joints
Engineering Computations. 2020;37(8):2895-2911   Crossref logo
Link1 Link2

Strength analysis of single lap dissimilar materials bolted joint
IOP Conference Series: Materials Science and Engineering. 2018;390:012022   Crossref logo
Link1 Link2 Link3 Link4

Optimization of Tensile Strength during Ultrasonic Lap Welding of Dissimilar Metals Using Taguchi’s Philosophy
Applied Mechanics and Materials. 2014;592-594:652-657   Crossref logo
Link1

Tensile Stress Analyses through Digital Image Correlation of Single Lap Joints of High Strength Steel and Aluminum Alloy Using Adhesive Bonding
Materials Science Forum. 2016;879:363-368   Crossref logo
Link1

On the Bead Geometry of Dissimilar Joints between SA516Gr65 and 304L Produced by TIG and A-TIG Welding
Materials Science Forum. 2016;863:19-22   Crossref logo
Link1

The influence of notching and mixed-adhesives at the bonding area on the strength and stress distribution of dissimilar single-lap joints
Composite Structures. 2020;241:112136   Crossref logo
Link1 Link2

Failure Analysis of Laminates Single-Lap Adhesive Joints under Uniaxial Tensile Loading
Advanced Materials Research. 2012;490-495:2201-2204   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.