Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Effect of EN Pulsing Ratio and Repetition Frequency on the Bead Appearance and Microstructure Evolution in Aluminum Welding using Variable Polarity GMAW
Minjung Kang, Jason Cheon, Tae Hyun Lee
JWJ. 2021;39(2):174-181.   Published online 2021 April 13    DOI: https://doi.org/10.5781/JWJ.2021.39.2.6

Excel Download

The Effect of EN Pulsing Ratio and Repetition Frequency on the Bead Appearance and Microstructure Evolution in Aluminum Welding using Variable Polarity GMAW
Journal of Welding and Joining. 2021;39(2):174-181   Crossref logo
Link1 Link2 Link3

Effect of wire feed rate on microstructure development during bead on plate welding of microalloyed steel using P-GMAW
Materials Today: Proceedings. 2021;42:423-428   Crossref logo
Link1 Link2

Effect of Polarity and Oxide Fluxes on Weld-bead Geometry in Activated Tungsten Inert Gas (A-TIG) Welding
Journal of Welding and Joining. 2020;38(4):380-388   Crossref logo
Link1 Link2 Link3

Effect of post weld heat treatment on the microstructure and corrosion behavior of AA2219 aluminum alloy joints welded by variable polarity tungsten inert gas welding
Materials & Design (1980-2015). 2015;65:1075-1082   Crossref logo
Link1 Link2

Effects of Welding Speed and Pulse Frequency on Surface Depression in Variable Polarity Gas Tungsten Arc Welding of Aluminum Alloy
Metals. 2019;9(2):114   Crossref logo
Link1

Welding of Aluminium Alloy Thin Sheets Using Variable Polarity MIG Method
Solid State Phenomena. 2013;211:15-22   Crossref logo
Link1

Effect of Current on Mechanical Properties and Microstructure of Aluminum 6061 with Gas Tungsten Arc Welding Process
Kapal: Jurnal Ilmu Pengetahuan dan Teknologi Kelautan. 2020;17(3):107-113   Crossref logo
Link1 Link2

Welding polarity effects on weld spatters and bead geometry of hyperbaric dry GMAW
Chinese Journal of Mechanical Engineering. 2015;29(2):351-356   Crossref logo
Link1 Link2 Link3

Mathematical modeling of effect of polarity on weld bead geometry in submerged arc welding
Journal of Manufacturing Processes. 2016;21:14-22   Crossref logo
Link1 Link2

Numerical calculation of variable polarity keyhole plasma arc welding process for aluminum alloys based on finite difference method
Computational Materials Science. 2007;40(2):213-225   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.