Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Optimization of Direct Energy Deposition of 304L Stainless Steel through Laser Process Parameters
SeongSeon Shin, Sung-Min Kwon, ChiYen Kim, JongHoon Lee, JunHo Hwang, HyunDeok KIm
JWJ. 2021;39(2):182-188.   Published online 2021 April 7    DOI: https://doi.org/10.5781/JWJ.2021.39.2.7

Excel Download

Optimization of Direct Energy Deposition of 304L Stainless Steel through Laser Process Parameters
Journal of Welding and Joining. 2021;39(2):182-188   Crossref logo
Link1 Link2 Link3

Optimization of laser welding process parameters in dissimilar joint of stainless steel AISI316/AISI1018 low carbon steel to attain the maximum level of mechanical properties through PWHT
Optics & Laser Technology. 2019;112:314-322   Crossref logo
Link1 Link2

Directed Energy Deposition of AISI 316L Stainless Steel Powder: Effect of Process Parameters
Metals. 2021;11(6):932   Crossref logo
Link1

Optimization of Process Parameters in TIG Welded Joints of AISI 304L -Austenitic Stainless Steel using Taguchi’s Experimental Design Method
Materials Today: Proceedings. 2019;16:1188-1195   Crossref logo
Link1 Link2

Optimization of pulsed GTA welding process parameters for the welding of AISI 304L stainless steel sheets
The International Journal of Advanced Manufacturing Technology. 2008;40(5-6):478-489   Crossref logo
Link1 Link2 Link3

Effect of processing parameters on microstructure and tensile properties of austenitic stainless steel 304L made by directed energy deposition additive manufacturing
Acta Materialia. 2016;110:226-235   Crossref logo
Link1 Link2

Optimization of pulsed laser welding process parameters in order to attain minimum underfill and undercut defects in thin 316L stainless steel foils
Optics & Laser Technology. 2018;99:30-38   Crossref logo
Link1 Link2

Functional composite metal for WC-dispersed 304L stainless steel matrix composite with alloying by direct laser: Microstructure, hardness and fracture toughness
Vacuum. 2015;121:96-104   Crossref logo
Link1 Link2

Monitoring and analysis of melt-assisted deformation behavior of 304L stainless steel during multipass laser forming process using IR pyrometer and laser-based displacement sensor
Optics & Laser Technology. 2021;135:106718   Crossref logo
Link1 Link2

Optimization of process parameters for solid and porous steel alloy structures produced by direct metal deposition
Materials Today: Proceedings. 2017;4(8):8918-8927   Crossref logo
Link1 Link2