Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Aluminum Arc Butt Joint Weld Geometry on Fatigue Strength
Jungho Cho, Sungjin Baek, Seungchul Shin, Gunho Lee, Mun-Gu Kang, Young-Rae Jo
J Weld Join. 2021;39(1):103-108.   Published online 2021 February 22    DOI: https://doi.org/10.5781/JWJ.2021.39.1.12

Excel Download

Effect of Aluminum Arc Butt Joint Weld Geometry on Fatigue Strength
Journal of Welding and Joining. 2021;39(1):103-108   Crossref logo
Link1 Link2 Link3

Experimental characterization of fatigue strength in butt welded joint considering the geometry and the effect of cooling rate of the weld
Journal of Physics: Conference Series. 2017;843:012047   Crossref logo
Link1 Link2 Link3 Link4

Effect of weld geometry on fatigue performance of 6061-T6 aluminum GMAW: part 1. Butt joint
Journal of Mechanical Science and Technology. 2022;36(10):5201-5208   Crossref logo
Link1 Link2 Link3

Effect of residual stress redistribution and weld reinforcement geometry on fatigue crack growth of butt welded joints
International Journal of Fatigue. 2020;139:105780   Crossref logo
Link1 Link2

Effect of Lack of Penetration on the fatigue strength of high strength steel butt weld
KSME Journal. 1994;8(2):191-197   Crossref logo
Link1 Link2 Link3 Link4

The Effect of Weld Reinforcement and Post-Welding Cooling Cycles on Fatigue Strength of Butt-Welded Joints under Cyclic Tensile Loading
Materials. 2018;11(4):594   Crossref logo
Link1

Effect of weld toe geometry on fatigue life of lap fillet welded ultra-high strength steel joints
International Journal of Fatigue. 2018;116:409-420   Crossref logo
Link1 Link2

Influence of weld quality on the fatigue strength of thin normal and high strength steel butt joints
Welding in the World. 2016;60(4):731-740   Crossref logo
Link1 Link2 Link3

On the effect of weld defects on the fatigue strength of beam welded butt joints
Procedia Structural Integrity. 2018;13:2053-2058   Crossref logo
Link1 Link2

Effect of joint clearance on fatigue strength of brazed jointSasabe, K.Q. J. Jpn. Weld. Soc. May 1989 7, (2), 98–102 (in Japanese)
International Journal of Fatigue. 1990;12(3):224-224   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.