Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Modeling of Laser Welds Using Machine Learning Algorithm Part II: Geometry and Mechanical Behaviors of Laser Overlap Welded High Strength Steel Sheets
Hyeonjeong You, Minjung Kang, Sung Yi, Soongkeun Hyun, Cheolhee Kim
J Weld Join. 2021;39(1):36-44.   Published online 2021 February 15    DOI: https://doi.org/10.5781/JWJ.2021.39.1.4

Excel Download

Modeling of Laser Welds Using Machine Learning Algorithm Part II: Geometry and Mechanical Behaviors of Laser Overlap Welded High Strength Steel Sheets
Journal of Welding and Joining. 2021;39(1):36-44   Crossref logo
Link1 Link2 Link3

Modeling of Laser Welds Using Machine Learning Algorithm Part I: Penetration Depth for Laser Overlap Al/Cu Dissimilar Metal Welds
Journal of Welding and Joining. 2021;39(1):27-35   Crossref logo
Link1 Link2 Link3

Tensile–Shear Fracture Behavior Prediction of High-Strength Steel Laser Overlap Welds
Metals. 2018;8(5):365   Crossref logo
Link1

Failure mode of laser welds in lap-shear specimens of high strength low alloy (HSLA) steel sheets
Fatigue & Fracture of Engineering Materials & Structures. 2011;35(3):219-237   Crossref logo
Link1 Link2

Fatigue Strength and Damage Mechanisms of Laser Welded Structural Carbon Steel Sheets
Key Engineering Materials. 2015;662:201-204   Crossref logo
Link1

Metallurgical and Mechanical Characterization of Laser Spot Welded Low Carbon Steel Sheets
steel research international. 2010;81(12):1144-1150   Crossref logo
Link1 Link2

Microstructure and mechanical behavior of Nd:YAG laser beam welded high strength low alloy steel joints
Optik. 2020;208:164050   Crossref logo
Link1 Link2

Laser beam and laser‐GMAW‐hybrid welded joints made of high‐strength fine‐grained structural steels
Steel Construction. 2022;15(3):195-195   Crossref logo
Link1 Link2

Evaluation of Microstructure and Selected Mechanical Properties of Laser Beam Welded S690QL High-Strength Steel
Advances in Materials Science. 2018;18(3):34-42   Crossref logo
Link1 Link2

Bending Strength of Laser-Welded Sandwich Steel Panels of Ultra-High Strength Steel
Key Engineering Materials. 2018;786:286-292   Crossref logo
Link1