Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
A Study for Brittle Crack Prevention and Fatigue Life Improvement using a Welded Stiffener
Tae-Woo Kang, Myung-Hyun Kim
J Weld Join. 2018;36(6):28-33.   Published online 2018 December 26    DOI: https://doi.org/10.5781/JWJ.2018.36.6.5

Excel Download

A Study for Brittle Crack Prevention and Fatigue Life Improvement using a Welded Stiffener
Journal of Welding and Joining. 2018;36(6):28-33   Crossref logo
Link1 Link2 Link3

Study on fatigue behavior and crack propagation life of longitudinal fillet welded lap joint
International Journal of Fatigue. 2022;107301   Crossref logo
Link1 Link2

Fatigue crack growth in brittle solids
Fatigue of Materials. 1998;383-407   Crossref logo
Link1

Rapid method for low cycle fatigue properties: thickness effect on the fatigue crack initiation life of welded joints
Fatigue & Fracture of Engineering Materials & Structures. 2015;38(12):1492-1506   Crossref logo
Link1 Link2

Fatigue Damage Analysis on Crack Growth and Fatigue Life of Welded Bridge Members with Initial Crack
Key Engineering Materials. 2006;324-325:251-254   Crossref logo
Link1

CRACK TIP PARAMETERS FOR CREEP-BRITTLE CRACK GROWTH
Fatigue & Fracture of Engineering Materials & Structures. 2002;21(4):387-401   Crossref logo
Link1 Link2

Fatigue Crack Propagation Experiment and Remaining Fatigue Life Evaluation for Welded Crane Members with Initial Crack
Advanced Materials Research. 2013;823:137-142   Crossref logo
Link1

Fatigue crack growth characteristics of inertia friction welded Ti17 alloy
Fatigue & Fracture of Engineering Materials & Structures. 2013;37(1):39-49   Crossref logo
Link1 Link2

Increasing fatigue crack initiation life in butt-welded UIC60 rail by optimization of welding process parameters
International Journal of Fatigue. 2021;151:106367   Crossref logo
Link1 Link2

A study on fatigue life in butt-welded joints containing surface crack under non-constant spectrum loadingZhao, J. and Huang, W. International Journal of Pressure Vessels and Piping (1997) 70, 117–120
International Journal of Fatigue. 1998;20(1):78-78   Crossref logo
Link1 Link2