Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Solidification Cracking Behavior in Austenitic Stainless Steel Laser Welds (Part 2) -Effects of δ-ferrite Crystallization and Solidification Segregation Behavior on Solidification Cracking Susceptibility- |
Eun-Joon Chun, Su-Jin Lee, Jeong Suh, Namhyun Kang, Kazuyoshi Saida |
J Weld Join. 2016;34(5):61-69. Published online 2016 October 30 DOI: https://doi.org/10.5781/JWJ.2016.34.5.61 |
Evaluation of Solidification Cracking Susceptibility in Austenitic Stainless Steel Welds Using Laser Beam Welding Transverse-Varestraint Test Solidification Cracking Studies in Multi Pass Laser Hybrid Welding of Thick Section Austenitic Stainless Steel Solidification Cracking Susceptibility in C-Mn Steel CO2 Laser Welds Solidification cracking in austenitic stainless steel welds Evaluation of solidification cracking susceptibility in laser welds for type 316FR stainless steel Weld Solidification Cracking in 304 to 304L Stainless Steel Characterization of Solidification Cracking in 304HCu Austenitic Stainless Steel Welds Solidification cracking in duplex stainless steel flux-cored arc welds Part 2 — susceptibility of 22Cr all-weld metals under high restraint Effect of sulfur, phosphorus, silicon, and delta ferrite on weld solidification cracking of AISI 310S austenitic stainless steel Solidification and solidification cracking in nitrogen-strengthened austenitic stainless steels |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |