Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effects of laser power on hardness and microstructure of the surface melting hardened SKD61 hot die steel using Yb:YAG disk laser
Kwang-Hyeon Lee, Seong-Won Choi, Chung-Yun Kang
J Weld Join. 2015;33(3):54-61.   Published online 2015 June 30    DOI: https://doi.org/10.5781/JWJ.2015.33.3.54

Excel Download

Effect of laser power and powder feeding on the microstructure of laser surface alloying hardened H13 steel using SKH51 powder
Materials & Design. 2016;95:173-182   Crossref logo
Link1 Link2

Welding of Thermomechanically Rolled Steel by Yb:YAG Disk Laser / Spawanie Stali Walcowanej Termomechanicznie Laserem Dyskowym Yb:YAG
Archives of Metallurgy and Materials. 2015;60(4):2851-2860   Crossref logo
Link1 Link2

A comparative study on surface topography and micro hardness of laser polished hardened AISI D2 tool steel
. 2021;   Crossref logo
Link1 Link2

CoCr alloy processed by Selective Laser Melting (SLM): effect of Laser Energy Density on microstructure, surface morphology, and hardness
Journal of Manufacturing Processes. 2020;52:106-119   Crossref logo
Link1 Link2

Analysis of Residual Stress Distribution and Corrosion in Laser Surface Hardened Low Alloy Steel with a Flat Top-Hat Laser Beam, Using a High-Power Diode Laser
Arabian Journal for Science and Engineering. 2022;   Crossref logo
Link1 Link2 Link3

Microstructure and wear resistance of Stellite-6/WC MMC coatings produced by laser cladding using Yb:YAG disk laser
International Journal of Refractory Metals and Hard Materials. 2016;58:157-164   Crossref logo
Link1 Link2

Microstructure and properties of borided 41Cr4 steel after laser surface modification with re-melting
Applied Surface Science. 2003;214(1-4):278-288   Crossref logo
Link1 Link2

Laser controlled melting of H12 hot-work tool steel with B4C particles at the surface
Optics & Laser Technology. 2015;74:36-42   Crossref logo
Link1 Link2

Microstructure, chemical composition and properties of the surface layer of M2 steel after laser melting under different conditions
Applied Surface Science. 1995;86(1-4):317-322   Crossref logo
Link1 Link2

Microstructure evolution of WC/steel composite by laser surface re-melting