Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effects of Average Power on Laser Cladding of Hypereutectic Al-Si Alloy on Al 1050 Alloy
Hyoung-Keun Lee
JWJ. 2011;29(2):88-93.   Published online 2011 May 7

Excel Download

Effects of Rotating Magnetic Field on Microstructure and Properties of Bi-Containing Hypereutectic Al-Si Alloy
Advanced Materials Research. 2015;1120-1121:1119-1123   Crossref logo
Link1

Method for making hypereutectic Al-Si alloy composite materials
Composites. 1991;22(2):167   Crossref logo
Link1 Link2

A New Al-ZnS Master Alloy Designed for Modifying Hypereutectic Al-Si Alloy and its Refinement Performance on Primary Si
Advanced Materials Research. 2015;1088:242-244   Crossref logo
Link1

Effect of Al–5Ti–C Master Alloy on the Microstructure and Mechanical Properties of Hypereutectic Al–20%Si Alloy
Materials. 2014;7(2):1188-1200   Crossref logo
Link1

Microstructure Research of Magnesium with Laser Surface Cladding by Al-Si Alloy
Advanced Materials Research. 2011;291-294:1369-1372   Crossref logo
Link1

Refinement of hypereutectic Al–Si alloy by a new Al–Zr–P master alloy
Journal of Alloys and Compounds. 2010;503(2):L26-L30   Crossref logo
Link1 Link2

Complex modification of hypereutectic Al-Si alloy by a new Al-Y-P master alloy
Metals and Materials International. 2015;21(4):646-651   Crossref logo
Link1 Link2 Link3

Refinement of Primary Silicon Crystals by Novel Al-ZnS Master Alloy in Solidification of Hypereutectic Al-Si Alloys
Light Metals 2016. 2016;271-273   Crossref logo
Link1

Refinement of Hypereutectic Al–Si Alloy by a New Al–Sc–P Master Alloy
Journal of Inorganic and Organometallic Polymers and Materials. 2011;22(1):64-69   Crossref logo
Link1 Link2 Link3

Laser Surface Cladding of Al-Si Alloy
Key Engineering Materials. 2005;297-300:2813-2818   Crossref logo
Link1