Review on Ultrasonic and Laser Welding Technologies of Multi-Layer Thin Foils for the Lithium-Ion Pouch Cell Manufacturing
Musung Kim, Heeseon Bang, Soongkeun Hyun, Sung Yi, Cheolhee Kim
J Weld Join. 2023;41(6):462-474. Published online 2023 Dec 31 DOI: https://doi.org/10.5781/JWJ.2023.41.6.6
|
Citations to this article as recorded by
Quality Classification of Multi-Layer Copper Foil Stacks Welds for Ultrasonic Welding Using CNN and RNN
Seon-myoung Hong, Jae-woo Cho, Hee-seon Bang
Journal of Welding and Joining.2024; 42(5): 514. CrossRef
|